Alloy Steel Seamless Pipes ASTM A213 T11 Cold Drawn Boiler Tube Hot / Cold Finished
ASME SA213 Grade T11 alloy steel seamless tubes are known as chrome moly tubes. ASME specification alloy steel tubes are used for high temperature service applications. Seamless alloy steel tubes according to ASME SA 213 Grade T11 are reheated and furnished in full annlealed,isothermal annealed or normalized quenched and tempered condition. ASME SA 213 Grade T11 Alloy Steel Seamless Tubes have a typical chemistry with additions of 4.00-6.00 Chromium and 0.45-0.65 Molybdenum. Bearing minimum tensile strength of 415 Mpa ASME SA 213 Grade T11 Tubes have minimum yield strength of 205 Mpa. Seamless Tubes have a typical chemistry with additions of 4.00-6.00 Chromium and 0.45-0.65 Molybdenum. Bearing minimum tensile strength of 415 Mpa ASME SA 213 Grade T11 Tubes have minimum yield strength of 205 Mpa.
1. Ordering Information
Quantity (feet, meters, or number of lengths),
Name of material (seamless tubes),
Grade (T11),
Condition (hot finished or cold finished),
Size (outside diameter and minimum wall thickness),
Length (specific or random),
Hydrostatic Test or Nondestructive Electric Test
Increased Sulfur, and
Special requirements and any supplementary requirements selected.
2. Available Size Range
OD | Thickness | ||
mm | inch | mm | SCH |
88.9~141.3 | 3''~ 5'' | 2.11~19.05 | SCH10~XXS |
*If the steel grades and size you are looking for are not listed above, please contact us for further information. |
3. Standards:
ASTM A213 Standard Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes
4. Application:
Power plant; Boilers; Heat-Exchangers; Chemical Fertilizer; Petrochemicals; Offshore Oils; Gas Productions; Refineries and etc.
5. Chemical Requirements
Chemical Requirements | |||||||||
Grade | UNS Designation | Composition, % | |||||||
C | Mn | p | S | Si | Cr | Mo | Other Elements | ||
max | max | ||||||||
T11 | K11597 | 0.05-0.15 | 0.30-0.60 | 0.025 | 0.025 | 0.50-1.00 | 1.00-1.50 | 0.44-0.65 |
6. Mechanical Properties
Tensile Strength min: 60ksi/415MPa
Yield Strength min: 30ksi/205MPa
7. Heat Treatment Requirements
Heat Treatment Requirements | |||||
Grade | UNS Number | Heat Treat Type | Austenitizing/Solutioning Temperature min or range | Cooling Media | Subcritical Annealing or Tempering Temperature min or range °F 【°C】 |
T11 | K11597 | full or isothermal anneal normalize and temper | … | … | 1200°F【650°C】 |